In the initial PR for PP-71 I only cleaned up material_final_print_temperatures, but now the material_initial_print_temperatures are also coming into play, so I cleaned those as well. From research for PP-123 I know this is a safe change. Due to this cleanup the cool_min_temperature can now always follow the ultimaker default settings.
2023-02-09 14:28:11 +01:00

30 lines
771 B
INI

[general]
definition = ultimaker_s3
name = Fast - Experimental
version = 4
[metadata]
is_experimental = True
material = generic_pla
quality_type = draft
setting_version = 21
type = quality
variant = CC 0.6
weight = -2
[values]
gradual_infill_step_height = =3 * layer_height
infill_pattern = ='zigzag' if infill_sparse_density > 80 else 'triangles'
machine_nozzle_cool_down_speed = 0.75
machine_nozzle_heat_up_speed = 1.6
material_print_temperature = =default_material_print_temperature + 10
prime_tower_enable = True
speed_print = 45
speed_topbottom = =math.ceil(speed_print * 35 / 45)
speed_wall = =math.ceil(speed_print * 40 / 45)
speed_wall_0 = =math.ceil(speed_wall * 35 / 40)
speed_wall_x = =speed_wall
support_angle = 70
top_bottom_thickness = =layer_height * 4