Cura/resources/quality/ultimaker_s3/um_s3_aa0.4_cpe-plus_0.06mm.inst.cfg
Rijk van Manen 9088ab23f4 cleanup initial print temperatures
In the initial PR for PP-71 I only cleaned up material_final_print_temperatures, but now the material_initial_print_temperatures are also coming into play, so I cleaned those as well. From research for PP-123 I know this is a safe change. Due to this cleanup the cool_min_temperature can now always follow the ultimaker default settings.
2023-02-09 14:28:11 +01:00

36 lines
876 B
INI

[general]
definition = ultimaker_s3
name = Extra Fine
version = 4
[metadata]
material = generic_cpe_plus
quality_type = high
setting_version = 21
type = quality
variant = AA 0.4
weight = 1
[values]
infill_overlap = 0
infill_wipe_dist = 0
machine_min_cool_heat_time_window = 15
machine_nozzle_cool_down_speed = 0.85
machine_nozzle_heat_up_speed = 1.5
material_print_temperature = =default_material_print_temperature + 2
multiple_mesh_overlap = 0
prime_tower_enable = True
prime_tower_wipe_enabled = True
retraction_hop = 0.2
retraction_hop_enabled = False
retraction_hop_only_when_collides = True
retraction_prime_speed = =retraction_speed
skin_overlap = 20
speed_print = 40
speed_topbottom = =math.ceil(speed_print * 30 / 35)
speed_wall = =math.ceil(speed_print * 35 / 40)
speed_wall_0 = =math.ceil(speed_wall * 30 / 35)
support_z_distance = =layer_height
wall_0_inset = 0